Stainless Steel 15-5
Material Notes: Stainless Steel 15-5 is a precipitation-hardening martensitic stainless steel which exhibits good corrosion resistance as well as transverse properties. This grade is appropriate for applications in which strength and toughness can be designed by controlling the temperate range during heat treatment.
Applications: Valves, Parts of the Aircraft, Gears, Pump Components.
Specifications for Stainless Steel 15-5
| Parameter | Value |
|---|---|
| Chemical Composition | |
| Iron (Fe) | 71.91% - 79.85% |
| Chromium (Cr) | 14.0% - 15.5% |
| Nickel (Ni) | 3.5% - 5.5% |
| Copper (Cu) | 2.5% - 4.5% |
| Manganese (Mn) | 1.0% max |
| Silicon (Si) | 1.0% max |
| Carbon (C) | 0.07% max |
| Phosphorus (P) | 0.04% max |
| Sulfur (S) | 0.03% max |
| Niobium + Tantalum (Nb + Ta) | 0.15% - 0.45% |
| Mechanical Properties | |
| Tensile Strength | 1380 MPa (200,000 psi) |
| Yield Strength | 1275 MPa (184,900 psi) |
| Elastic Modulus | 196 GPa (28,427 ksi) |
| Elongation at Break | 10% |
| Hardness (Brinell) | 420 |
| Hardness (Rockwell C) | 44.2 |
| Thermal Properties | |
| Thermal Expansion Coefficient | 10.4 µm/m°C |
| Thermal Conductivity | 17.8 W/mK |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get 15-5 Stainless Steel CNC machining parts from Hopeful
Hopeful’s China factory is just the place for you if you desire premium CNC machining parts out of grade stainless steel! From aerospace to automotive, our Stainless Steel 15-5 parts are highly versatile and perfectly suitable for a variety of applications. You can always count on our high end manufacturing processes to provide the best products available. So contact us today to boost your engineering projects with our parts.