AISI 12L14 Steel
Material Notes: AISI 12L14 Steel is categorized as a low-carbon alloy and it is known for its exceptional machinability due to the addition of lead which reduces tool wear. It has a tensile strength of 540 megapascals and a yield strength of 415 mega pascals which makes this steel a good fit for non-critical applications with low-difficulty machining requirements and moderate strength.
Applications: The AISI 12L14 steel is suited perfectly for precision components, automotive parts, and industrial fittings due to its excellent machinability. Its effectiveness in mass production lowers the costs and prolongs the lifespan of the tooling which makes it a dependable material for parts with strict tolerances and excellent surface finishes.
Specifications for AISI 12L14 Steel
AISI 12L14 steel is a free-machining alloy known for its excellent machinability, smooth finish, and strength. Widely used in manufacturing, it’s valued for its efficiency and versatility in industrial applications.
| Property | Metric | English | Comments |
|---|---|---|---|
| Density | 7.87 g/cc | 0.284 lb/in³ | Typical for steel. |
| Hardness, Brinell | 163 | 163 | |
| Hardness, Knoop | 184 | 184 | Converted from Brinell |
| Hardness, Rockwell B | 84 | 84 | Converted from Brinell |
| Hardness, Vickers | 170 | 170 | Converted from Brinell |
| Tensile Strength, Ultimate | 540 MPa | 78300 psi | |
| Tensile Strength, Yield | 415 MPa | 60200 psi | |
| Elongation at Break | 10% | 10% | |
| Reduction of Area | 35% | 35% | |
| Modulus of Elasticity | 200 GPa | 29000 ksi | Typical for steel |
| Bulk Modulus | 160 GPa | 23200 ksi | Typical for steel. |
| Poisson's Ratio | 0.29 | 0.29 | Typical for steel |
| Machinability | 160% | 160% | Based on 100% machinability for AISI 1212 steel. |
| Shear Modulus | 80.0 GPa | 11600 ksi | Typical for steel. |
| Electrical Resistivity | 0.0000174 ohm-cm | 0.0000174 ohm-cm | Typical steel |
| CTE, linear @ 20°C/68°F | 11.5 µm/m-°C | 6.39 µin/in-°F | Typical steel |
| CTE, linear @ 0-300°C/32-572°F | 12.2 µm/m-°C | 6.78 µin/in-°F | Typical for steel |
| CTE, linear @ 0-500°C/32-932°F | 13.9 µm/m-°C | 7.72 µin/in-°F | Typical for steel |
| Specific Heat Capacity | 0.472 J/g-°C | 0.113 BTU/lb-°F | Typical steel |
| Thermal Conductivity | 51.9 W/m-K | 360 BTU-in/hr-ft²-°F | Typical steel |
| Carbon, C | <= 0.15 % | <= 0.15 % | |
| Iron, Fe | 97.91 - 98.7 % | 97.91 - 98.7 % | As remainder |
| Lead, Pb | 0.15 - 0.35 % | 0.15 - 0.35 % | |
| Manganese, Mn | 0.85 - 1.15 % | 0.85 - 1.15 % | |
| Phosphorus, P | 0.040 - 0.090 % | 0.040 - 0.090 % | |
| Sulfur, S | 0.26 - 0.35 % | 0.26 - 0.35 % |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get AISI 12L14 Steel CNC machining parts from Hopeful
Are you in search of unique precision steel machined components from AISI 12L14 steel? As one of the leading factories in China, we work with a wide range of industries, including automotive and aerospace, and produce the highest quality CNC machining precision pieces. Our clients appreciate the durability and machining accuracy of our AISI 12L14 steel parts. Make your bulk purchases now and enjoy quantity discounts. Reach out to us now to order and witness for yourself the quality and professionalism we at Hopeful are proud of.