POM-C ESD
Key Features and Benefits: The POM-C ESD is a robust acetal copolymer developed for use in applications that necessitate antistatic features. Its blends of mechanical strength, thermal resistance (from 100°C to 140°C), and reliability make it suitable for semiconductor manufacturing as well as high-temperature, high-stress environments.
Applications: The POM-C ESD is suitable for very precise and robust industries like semiconductors, aviation, and vacuum technologies. It guarantees stable non-conductive performance in cleanrooms, serves aviation components e.g. engine parts and fuel systems, and provides reliable wear resistance in vacuum systems.
Specifications for POM-C ESD
This table presents for convenient reference the mechanical, thermal, and electrical properties, as well as some common applications of the referenced materials.
| Property | Value | Unit |
|---|---|---|
| Mechanical Properties | ||
| Yield strength | 45 | MPa |
| Elongation at break | 40 - 50 | % |
| Thermal Properties | ||
| Maximum service temperature | 100 to 140 | °C |
| Thermal expansion coefficient | 10 - 13 | 10^-6/°C |
| Thermal conductivity | 0.3 | W/(m⋅°C) |
| Electrical Properties | ||
| Electrical resistivity | 10 | μΩ*cm |
| Common Applications | ||
| Tool carriers | ||
| Housing parts | ||
| Rollers |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get POM-C ESD CNC machining parts from Hopeful
Are you searching for premium POM-C ESD CNC components in China? Hopeful has you covered. Being a leading supplier in the market, we provide POM-C precision parts manufactured to the levels of quality and performance requirement. Our products serve a variety of industries from electronics to automotive to aerospace. For all your CNC machining part requirements, trust the experts at Hopeful.