Copper C110
Material Notes:Copper C110 or Electrolytic Tough Pitch possesses great electrical characteristics, with high conductivity grade of 100 IACS and is made of copper 99.9%. This substance is also excellently resistive to corrosion and has vast ductility, as well as great forming qualities, making it useful for electrical, plumbing and architectural applications and systems. Due to its machinability being only twenty percent, it is deemed to be low grade, but due to its applicability and wide range of suitability, it is commonly used.
Applications: Copper C110 is an alloy whose ease of work is complemented by its exceptional electrical and thermal conductivity, resistance to corrosion, and durability. The alloy is commonly employed in the following: electrical system components (wires, transformers), plumbing and HVAC system elements (pipes and systems), automotive components (brake lines and radiators), architectural elements (decorative elements and roofing), marine engineering apparatus such as heat exchangers and piping, as well as gas distribution associated with medical equipment.
Specifications for Copper C110
Copper C110 is a wonder material boasting superb conductivity, corrosion resistance, and thermal properties. It is widely applied in electronics, construction, manufacturing, and remains one of the preferred materials in technical and industrial applications.
| Property | Value |
|---|---|
| Typical Physical Properties | |
| Melting Point | 1083°C |
| Density | 8.94 g/cm³ |
| Specific Heat | 385 J/Kg °K |
| Thermal Conductivity | 399 W/m°C |
| Thermal Expansion Coefficient | 17.3 x 10⁻⁶ per °C (20 - 200°C) |
| Electrical Conductivity | 101.5% IACS |
| Electrical Resistivity | 0.017 microhm/m |
| Modulus of Elasticity | 118,000 Kg/mm² |
| Fabrication Properties | |
| Hot Working Temperature Range | 728 - 825°C |
| Hot Formability | Good |
| Cold Formability | Good |
| Cold Reduction Between Anneals | 70% max |
| Machinability Rating | 85 - 90% (free cutting brass=100) |
| Joining Methods | |
| Soldering | Excellent |
| Brazing | Excellent |
| Oxy-acetylene Welding | Good |
| Gas-shielded Arc Welding | Excellent |
| Resistance Welding: Spot and Seam Butt | Not recommended - Good |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get Copper C110 CNC machining parts from Hopeful
Are you in need of trustworthy and accurate Copper C110 CNC machining parts in China? Hopeful is just the company you need! We leverage high-tech machining equipment combined with our skilled personnel to guarantee amazing results. Whether academic or commercial, prototypes or mass order, we can help. Get in touch with us now for further details and details of your machining requirements.