Copper C101
Material Notes: C101, or Copper with Oxygen Free Electronic Copper, remains one of the highest grades of copper for use in technical applications as its production is done free of oxygen and contaminants. Its purity reaches as high as 99.99% which yields remarkable conductivity with a value of 101% IACS.
Applications: Copper C101 is a high-purity copper that is highly sought after due to its superb heat and electricity conduction. It is widely utilized in electrical sectors and inother fields that demand precision. C101 is perfectly suited for connectors, wiring, transformers, motors, and even heat exchangers.
Specifications for Copper C101
In the below table technical details are presented which depict that the Copper C101 has high purity, good electrical conductivity and mechanical properties which enables it to be used for a number of applications.
| Parameter | Value/Description |
|---|---|
| Chemical Composition | Copper (Cu): 99.99%, Oxygen: 0.0005% |
| Tensile Strength | 200-360 MPa (43,500 PSI) |
| Proof Stress | 50-340 MPa |
| Elongation | 50-5% |
| Hardness | 40-110 HV (Rockwell B40) |
| Density | 8.92 g/cm³ |
| Melting Point | 1083 °C |
| Modulus of Elasticity | 117 GPa |
| Electrical Resistivity | 0.171 x 10⁻⁶ Ω.m |
| Thermal Conductivity | 391.1 W/m.K |
| Thermal Expansion | 16.9 x 10⁻⁶ /K |
| Corrosion Resistance | Good to excellent in most environments, except those containing ammonia ions |
| Machinability | Rating of 20 (compared to Alloy 360 FC Brass at 100) |
| Welding | Excellent for soldering; good for brazability and butt welding; fair for gas shielded arc welding |
| Applications | Connectors, transformers, general electronics, busbars, motor components, building fascias, heatsinks, cable strips |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get Copper C101 CNC machining parts from Hopeful
Looking for trustworthy and high-quality copper C101 CNC machining parts? Hopeful's China factory is a one-stop shop for everything regarding your CNC machining needs. Our C101 copper parts are professional-grade with uncompromised quality. Stop dealing with unfair markups from middlemen and get them from the source. Reach out to us today to place an order, and enjoy the quality and service we have to offer.