Intermediate Modulus Carbon Fiber
MaterialNotes: Intermediate Modulus Carbon Fiber is an economical material that is light, durable, and easy to handle. By weighing and efficing 42 – 47Msi and 800-1000ksi respectively, it meets and outperforms people’s expectations of standard fabrics, and is a whole lot cheaper relative to other high-quality materials.
Applications: Intermediate Modulus Carbon Fiber is a multi-functional material that possesses great strength, as well as thermal and flexural resistance. Used around the world, it serves components for aircraft, such as stabilizers and pressure vessels, industrial equipment like tools and tanks, and sport and recreation items like bicycles and fishing rods.
Specifications for Intermediate Modulus Carbon Fiber
Intermediate Modulus Carbon Fiber provides a high level of strength and stiffness combined with excellent versatility and thus, is particularly suited for use in high-aerospace, automotive, and sporting goods industries.
| Property | Metric | English | Comments |
|---|---|---|---|
| Density | 1.76 g/cc | 0.0636 lb/in³ | |
| Tensile Strength at Break | 5723 MPa | 830100 psi | |
| Elongation at Break | 1.90% | 1.90% | |
| Tensile Modulus | 279 GPa | 40500 ksi | at chord 6000-1000 |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get Intermediate Modulus Carbon Fiber CNC machining parts from Hopeful
Hopeful supplies the finest CNC machining parts of Intermediate Modulus Carbon Fiber in China. Our parts are meticulously crafted for a broad spectrum of applications, including automotive and aerospace industries. Rely on us to deliver your carbon fiber machining requirements with high quality products and customer service. Reach out to us and learn more about the rest of our product range, and how we can grow your business together.