H59 Brass
Material Notes: The H59 brass, which comprises 59-62% of copper and 38-40% of zinc, possesses malleability, corrosion resistance, and durability, which give it immense value. Its application is so extensive that it allows use in construction, automotive, and electrical engineering industries for components like fittings and valves. Due to its excellent workability coupled with thermal conductivity, the demand for H59 is expected to grow at 12% CAGR from 2025 to 2032.
Applications: H59 brass is a multipurpose material ranging from its strength, exemplary conductivity, and excellent machinability to its varied industrial use. Given its resistance to corrosion and excellent strength making it perfect for parts of machines such as bushings and gears, electrical components such as switches, plumbing fittings, decorative items like jewelry or even light fixtures.
Specifications for H59 Brass
| Property | H59 Brass |
|---|---|
| Tensile Strength | 380–630 MPa |
| Yield Strength | ~110 MPa |
| Hardness (Brinell) | 80–150 HB |
| Elongation at Break | 25%–45% |
| Density | ~8.5 g/cm³ |
| Melting Point | ~890–920°C |
| Electrical Conductivity | ~25% IACS (~14.5 MS/m) |
| Thermal Conductivity | ~120 W/m·K |
| Machinability Rating | ~30% (reference: free-cutting brass = 100%) |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get H59 Brass CNC machining parts from Hopeful
For quality CNC-machined H59 Brass parts, your best bet is with Hopeful. We make high-quality parts that solve your machining issues in a snap. Our factory, located in China, guarantees superior quality and precise parts. If you are looking for precision components for industrial equipment or need a special part for a project, custom-made H59 brass parts are the answer. Contact us now for information on ordering parts directly from our factory.