C3604 Brass
Material Notes:C3604 Brass is a 60-63% copper, 2.5-3.7% lead, and zinc alloy that boasts an exceptional blend of machinability and wear resistance. A higher lead content leads to better cutting performance, which makes it ideal for precision machining.
Applications:C3604 brass is broadly applied in the automotive, aerospace, and engineering industries for manufacturing components with precision. Its applications encompass fittings, valves, gears, and fasteners due to its excellent machining capabilities and mass production accuracy.
Specifications for C3604 Brass
The C3604 brass alloy has exceptional workability, longevity, and resistance to corrosion which makes it a widely used alloy in engineering and manufacturing. It can be machined into fine features components and many other objects.
| Property | Specification |
|---|---|
| Chemical Composition | Cu: 57.0-61.0%, Pb: 1.8-3.7%, Fe: <0.5%, Zn: Balance |
| Mechanical Properties | Tensile Strength: >335 N/mm², Vickers Hardness: 80 |
| Characteristics | Excellent machinability, corrosion resistance, good thermal and electrical conductivity |
| Applications | Precision components, electrical connectors, valves, fittings, decorative items |
| Standards | JIS: H3250 C3604, ASTM: C38000, DIN: CuZn39Pb3, GB: HPb60-2 |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get C3604 Brass CNC machining parts from Hopeful
C3604 offers you precision crafted C3604 brass components in China. We have a specialized team that deploys advanced techniques to guarantee high precision and quality for every single one of your machining projects. With us, you can be rest assured that all of your requirements and expectations will be surpassed.