C314 Brass
Material Notes: C314 brass, which is often called C31400 or leaded commercial bronze, is a wrought bronze alloy engineered for excellent strength, toughness, and precision. Its exact makeup is around 89% copper, 9% zinc, and 2% lead.
Applications:
• Acceptable within applicable limits for electrical connectors, terminals, and other conductive parts.
• Capable of producing precision screws, bolts, and other similar threaded articles.
• Multi-purpose working brass for bushing type and very broad machined valve components and other machinable parts.
• C314 Brass offers an optimal combination of machinability, conductivity, and corrosion resistance.
Specifications for C314 Brass
Widely accepted, C314 Brass is an alloy known for high machinability and dependable performance. Mostly comprised of copper and zinc, with traces of lead, it is a blend of strength, ductility, and corrosion resistance.
| Property | US Customary | Metric |
|---|---|---|
| Melting point - liquidus | 1900 °F | 1038 °C |
| Melting point - solidus | 1850 °F | 1010 °C |
| Density | 0.319 lb/in³ at 68 °F | 8.83 g/cm³ at 20 °C |
| Specific gravity | 8.83 | 8.83 |
| Electrical conductivity | 42% IACS at 68 °F | 0.246 MegaSiemens/cm at 20 °C |
| Thermal conductivity | 104 Btu/sq ft/ft hr/°F at 68 °F | 180 W/m at 20 °C |
| Coefficient of thermal expansion | 10.2 × 10⁻⁶ per °F (68-572 °F) | 17.6 × 10⁻⁶ per °C (20-300 °C) |
| Specific heat capacity | 0.09 Btu/lb/°F at 68 °F | 377.1 J/kg at 20 °C |
| Modulus of elasticity in tension | 17000 ksi | 117212 MPa |
| Modulus of rigidity | 6400 ksi | 44127 MPa |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get C314 Brass CNC machining parts from Hopeful
Are you in need of C314 Brass precision CNC machining components? Our factory has a wide range of modern equipment which allows us to produce highly specialized parts. No matter whether you require parts for bespoke industrial or commercial applications, we can help. Get C314 Brass CNC machine components from us and notice the difference in unparalleled accuracy and quality. Please consult us for pricing and delivery timelines.