Material Notes: C272 Brass, also called yellow brass, has high strength, malleability, and versatility. It contains zinc and copper – 62 to 65 percent of the former, and 34.6 to 38 percent of the latter, which form an alloy. In addition, this copper-zinc alloy has great formability, corrosion resistance, impressive electrical and thermal conductivity, and high tensile and yield strengths.
Applications: It is the strength, durability, and resistance of C272 Brass that makes it preferred by many industries. Its greatest demand comes from the manufacturing of fasteners, tubing, heat exchangers, pump parts, bearings, gears, and plumbing fittings such as couplings and valves.
Specifications for C272 Brass
C272 Steel is a highly adaptable alloy, prized for its strength and resistance to corrosion and tarnishing. Average usage in sectors such as automotive, construction, and electronics is attributed to its superb composition and mechanical properties.
| Property | Value |
|---|---|
| Melting Point - Liquidus (°F) | 1680 |
| Density (lb/cu in. at 68°F) | 0.305 |
| Specific Gravity | 8.44 |
| Electrical Conductivity (% IACS at 68°F) | 27.6 |
| Thermal Conductivity (Btu/sq ft/ft hr/°F at 68°F) | 67 |
| Coefficient of Thermal Expansion (10^-6 per °F, 68–572°F) | 11.4 |
| Specific Heat Capacity (Btu/lb/°F at 68°F) | 0.09 |
| Modulus of Elasticity in Tension (ksi) | 15000 |
| Modulus of Rigidity (ksi) | 5600 |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get C272 Brass CNC machining parts from Hopeful
In need of high grade C272 brass CNC machined components? Look no more! Hopeful has it all as we specialize in CNC machining. Top C272 Brass CNC machined components in China are effortlessly available from us so you can see the profits of the Hopeful distinction. Our talented specialists and advanced machinery allow us to produce the most advantageous components for your particular task. Call us to request a quote and we promise to turn your vision into a reality.