Brass C27400
Material Notes: Brass C27400, also known as Yellow Brass 63 by 37, is a copper and zinc alloy composited with 61 to 64% copper and minute proportions of lead and iron. This alloy is perfect for industrial and plumbing purposes due to its impeccable strength, workability, and corrosion-resistant properties. Some of the key properties that Brass C27400 shows are a tensile strength of about 74 ksi, yield strength of around 55 ksi, and maximum elongation of 10% in hard-drawn temper.
Applications: Brass C27400 is a multifaceted alloy with great utility in industrial and plumbing works. Its moderate strength, superb workability, and conductivity render it useful in cold-headed parts and specialty items.
Specifications for Brass C27400
C27400 brass alloy is distinguished by its corrosion resistance and strength making it capable of withstanding high pressure, and has good machinability.
| Property | Value |
|---|---|
| Melting Point - Liquidus (°F) | 1680 |
| Density (lb/cu in. at 68°F) | 0.305 |
| Specific Gravity | 8.44 |
| Electrical Conductivity (% IACS at 68°F) | 27.6 |
| Thermal Conductivity (Btu/sq ft/ft hr/°F at 68°F) | 67 |
| Coefficient of Thermal Expansion (10^-6 per °F, 68–572°F) | 11.4 |
| Specific Heat Capacity (Btu/lb/°F at 68°F) | 0.09 |
| Modulus of Elasticity in Tension (ksi) | 15000 |
| Modulus of Rigidity (ksi) | 5600 |
View our latest news
The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...
The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...
Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...
In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...
Get Brass C27400 CNC machining parts from Hopeful
CNC machined parts from Brass C27400 available? You are absolutely in the right place! We, Hopeful/Brass, are leaders in precision-engineered parts and the most reliable partner in China. Our CNC machining ensures that all your manufacturing products are made with exceptional quality. Place your order for our top quality Brass C27400 CNC machined parts and feel the change in quality and performance. Get in touch with us today!