# 304 Stainless Steel

**Material Notes:** The 304 grade of stainless steel is the basic ‘18/8 type’ of the family and it is well mastered for its scope of application and therefore available in a number of forms and finishes. It has superior welding properties thus making it a perfect choice for form or welding projects due to its balanced upper austenitic. 304 grade is widely used in various industrial, architectural, and transportation structures.

**Applications:** The products we manufacture and serve all have an application to stainless steel beer kegs, chemical equipment, dairy equipment, kitchen cooking tools, surgical implements used by hospitals, etc. Our dependable and adaptable materials guarantee optimal efficiency in kitchen sinks, pressure vessels, and more. Leverage us to deliver stainless steel products tailored to your requirements.

[contact us](#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjE2OTQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D)

- [Stainless Steel 304 PDF](https://hplmachining.com/wp-content/uploads/2025/01/Stainless-Steel-304-1.pdf)

Sam Sun - CNC Machining Expert：Our expertise is in CNC milling, CNC turning, 3D printing, urethane casting, and sheet metal fabrication that allows us to provide for you bespoke and high precision solutions.

![Sam Sun](https://hplmachining.com/wp-content/uploads/2025/01/2-9.webp)

Sam Sun

## Specifications for Stainless Steel 304

| ﻿Property | Metric | English | Comments |
| --- | --- | --- | --- |
| Density | 8.00 g/cc | 0.289 lb/in³ | |
| Hardness, Brinell | 123 | 123 | Converted from Rockwell B hardness. |
| Hardness, Knoop | 138 | 138 | Converted from Rockwell B hardness. |
| Hardness, Rockwell B | 70 | 70 | |
| Hardness, Vickers | 129 | 129 | Converted from Rockwell B hardness. |
| Tensile Strength, Ultimate | 505 MPa | 73200 psi | |
| Tensile Strength, Yield | 215 MPa @ Strain 0.2% | 31200 psi @ Strain 0.2% | |
| Elongation at Break | 70% | 70% | in 50 mm |
| Modulus of Elasticity | 193 GPa | 28000 ksi | |
| Poisson's Ratio | 0.29 | 0.29 | |
| Shear Modulus | 77.0 GPa | 11200 ksi | |
| Izod Impact | 150 J @ -195 °C | 111 ft-lb @ -319 °F | V-Notch |
|  | 150 J @ 21.0 °C | 111 ft-lb @ 69.8 °F | V-Notch |
| Charpy Impact | 325 J | 240 ft-lb | |
| Electrical Resistivity | 0.0000720 ohm-cm @ 20.0 °C | 0.0000720 ohm-cm @ 68.0 °F | |
|  | 0.000116 ohm-cm @ 650 °C | 0.000116 ohm-cm @ 1200 °F | |
| Magnetic Permeability | 1.02 | 1.02 | at RT |
| CTE, linear | 17.3 µm/m-°C @ 0-100 °C | 9.61 µin/in-°F @ 32-212 °F | |
|  | 17.8 µm/m-°C @ 0-315 °C | 9.89 µin/in-°F @ 32-599 °F | |
|  | 18.7 µm/m-°C @ 0-650 °C | 10.4 µin/in-°F @ 32-1200 °F | |
| Specific Heat Capacity | 0.500 J/g-°C @ 0-100 °C | 0.120 BTU/lb-°F @ 32-212 °F | |
| Thermal Conductivity | 16.2 W/m-K @ 0-100 °C | 112 BTU-in/hr-ft²-°F @ 32-212 °F | |
|  | 21.5 W/m-K @ 500 °C | 149 BTU-in/hr-ft²-°F @ 932 °F | |
| Melting Point | 1400 - 1455 °C | 2550 - 2651 °F | |
| Solidus | 1400 °C | 2550 °F | |
| Liquidus | 1455 °C | 2651 °F | |
| Carbon, C | <= 0.080% | <= 0.080% | |
| Chromium, Cr | 18 - 20% | 18 - 20% | |
| Iron, Fe | 66.345 - 74% | 66.345 - 74% | as balance |
| Manganese, Mn | <= 2.0% | <= 2.0% | |
| Nickel, Ni | 8.0 - 10.5% | 8.0 - 10.5% | |
| Phosphorus, P | <= 0.045% | <= 0.045% | |
| Silicon, Si | <= 1.0% | <= 1.0% | |
| Sulfur, S | <= 0.030% | <= 0.030% | |

Our Blog

## View our latest news

[![The Key Differences Between UHMW and HDPE Plastic Machining](https://hplmachining.com/wp-content/uploads/2025/01/3.6.png)](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

[January 9, 2025](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

[The Key Differences Between UHMW and HDPE Plastic Machining](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...

[Read More](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

[![3.1 1](https://hplmachining.com/wp-content/uploads/2025/01/3.1-1.webp)](https://hplmachining.com/blog/what-is-cnc-milling/)

[January 9, 2025](https://hplmachining.com/blog/what-is-cnc-milling/)

[Everything You Need to Know About CNC Milling: How a CNC Mill Works](https://hplmachining.com/blog/what-is-cnc-milling/)

The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...

[Read More](https://hplmachining.com/blog/what-is-cnc-milling/)

[![Why Are CNC Machines Important in Modern Manufacturing?](https://hplmachining.com/wp-content/uploads/2025/01/4.1.webp)](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

[January 9, 2025](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

[Understanding the Key Components of a CNC Machine](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...

[Read More](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

[![Unlocking the Mysteries: The Key Differences Between Metal Cutting and Machining Processes](https://hplmachining.com/wp-content/uploads/2025/01/1-12.webp)](https://hplmachining.com/blog/cutting-and-machining-metal/)

[January 9, 2025](https://hplmachining.com/blog/cutting-and-machining-metal/)

[Unlocking the Mysteries: The Key Differences Between Metal Cutting and Machining Processes](https://hplmachining.com/blog/cutting-and-machining-metal/)

In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...

[Read More](https://hplmachining.com/blog/cutting-and-machining-metal/)

![Get 304 Stainless Steel CNC machining parts from Hopeful](https://hplmachining.com/wp-content/uploads/2025/01/1-144.webp)

## Get 304 Stainless Steel CNC machining parts from Hopeful

Are you looking for quality parts made from CNC machining? 304 Stainless Steel parts created by Hopeful will provide you with the top standards you are looking for. The most modern CNC technologies with the utmost accuracy and strength ensure our 304 Stainless Steel parts are manufactured in our modern factory in China. Today's advanced machines have specialized components with increased operational life and improved overall quality. Get in touch with us now so we can process your order and your machinery performance greatly improves with the new parts from Hopeful.

[Get an Instant Quote](#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjE2OTQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D)

Scroll to Top

WhatsApp us

Get in touch with Kunshan Hopeful Metal Products Co.,Ltd

Contact Form used

Your Name \*

Email

Phone/WhatsApp

Your Message

File Upload

Please upload your processing drawings, we promise that the uploaded files will be confidential

Submit Form

```json
{"@context":"https://schema.org","@graph":[{"@type":"BreadcrumbList","@id":"https://hplmachining.com/services/cnc-machining/stainless-steel/stainless-steel-304/#breadcrumb","itemListElement":[{"@type":"ListItem","position":"1","item":{"@id":"https://hplmachining.com","name":"Home"}},{"@type":"ListItem","position":"2","item":{"@id":"https://hplmachining.com/services/","name":"Services"}},{"@type":"ListItem","position":"3","item":{"@id":"https://hplmachining.com/services/cnc-machining/","name":"CNC Machining Service"}},{"@type":"ListItem","position":"4","item":{"@id":"https://hplmachining.com/services/cnc-machining/stainless-steel/","name":"Stainless Steel CNC Machining Services"}},{"@type":"ListItem","position":"5","item":{"@id":"https://hplmachining.com/services/cnc-machining/stainless-steel/stainless-steel-304/","name":"Stainless Steel 304"}}]}]}
```