# Aluminum 6061-T6

**Material Notes**: General 6061 characteristics and uses: Good adhesive properties, good acceptance of applied coatings. It is readily available and combines moderate strength, ease of fabrication, and high corrosion resistance. A better chipping ability can be achieved with T8 and T9 tempers compared to T6 temper.

**Applications**: Aircraft fittings, camera lens mounts, couplings, marine fittings and hardware, electrical fittings and connectors, decorative or miscellaneous. Hardware, hinge pins, magneto parts, brake pistons, hydraulic pistons, appliance fittings, valves and valve parts, and bike frames.

[contact us](#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjE2OTQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D)

- [Aluminum 6061-T6 PDF](https://hplmachining.com/wp-content/uploads/2025/01/Aluminum-6061-T6-PDF.pdf)

Sam Sun - CNC Machining Expert：Our expertise is in CNC milling, CNC turning, 3D printing, urethane casting, and sheet metal fabrication that allows us to provide for you bespoke and high precision solutions.

![Sam Sun](https://hplmachining.com/wp-content/uploads/2025/01/2-9.webp)

Sam Sun

## Specifications for Aluminum 6061-T6 | 3.3211 | 65028 | AlMg1SiCu

This table contains all the necessary characteristics of matter; its physical, mechanical, electrical, and thermal dimensions as well as individual component properties. It will help in understanding the overall functionality of materials and their appropriateness to specific applications.

| ﻿Category | Property | Metric | English | Comments |
| --- | --- | --- | --- | --- |
| Physical Properties | Density | 2.70 g/cc | 0.0975 lb/in³ | AA; Typical |
| Mechanical Properties | Hardness, Brinell | 95 | 95 | AA; Typical; 500 g load; 10 mm ball |
|  | Hardness, Knoop | 120 | 120 | Converted from Brinell Hardness Value |
|  | Hardness, Rockwell A | 40 | 40 | Converted from Brinell Hardness Value |
|  | Hardness, Rockwell B | 60 | 60 | Converted from Brinell Hardness Value |
|  | Hardness, Vickers | 107 | 107 | Converted from Brinell Hardness Value |
|  | Tensile Strength, Ultimate | 310 MPa | 45000 psi | AA; Typical |
|  | Tensile Strength, Yield | 276 MPa | 40000 psi | AA; Typical |
|  | Modulus of Elasticity | 68.9 GPa | 10000 ksi | AA; Typical; Average of tension and compression. Compression modulus \~2% higher |
|  | Notched Tensile Strength | 324 MPa | 47000 psi | Specimen Kt = 17, side-notched |
|  | Ultimate Bearing Strength | 607 MPa | 88000 psi | Edge distance/pin diameter = 2.0 |
|  | Bearing Yield Strength | 386 MPa | 56000 psi | Edge distance/pin diameter = 2.0 |
|  | Fatigue Strength | 96.5 MPa | 14000 psi | Completely reversed stress, 5×10⁸ cycles |
|  | Fracture Toughness | 29.0 MPa-m½ | 26.4 ksi-in½ | KIC; TL orientation |
|  | Machinability | 50% | 50% | Scale of Aluminum Alloys (0-100) |
|  | Shear Modulus | 26.0 GPa | 3770 ksi | Estimated from similar Al alloys |
|  | Shear Strength | 207 MPa | 30000 psi | AA; Typical |
| Electrical Properties | Electrical Resistivity | 0.00000399 ohm-cm | 0.00000399 ohm-cm | AA; Typical; Temperature 20°C (68°F) |
| Thermal Properties | CTE, Linear | 23.6 µm/m-°C (20–100°C range) | 13.1 µin/in-°F (68–212°F range) | AA; Typical |
|  |  | 25.2 µm/m-°C (20–300°C range) | 14.0 µin/in-°F (68–572°F range) | |
|  | Specific Heat Capacity | 0.896 J/g-°C | 0.214 BTU/lb-°F | |
|  | Thermal Conductivity | 167 W/m-K | 1160 BTU-in/hr-ft²-°F | Typical at 77°F |
|  | Melting Point | 582–651.7 °C | 1080–1205 °F | Typical range for wrought products ≥ ¼ in. thickness |
| Processing Properties | Solution Temperature | 529 °C | 985 °F | |
|  | Aging Temperature | 160 °C, hold 18 hr | 320 °F, hold 18 hr | Rolled or drawn products |
|  |  | 177 °C, hold 8 hr | 350 °F, hold 8 hr | Extrusions or forgings |
| Component Elements | Aluminum, Al | 95.8–98.6% | 95.8–98.6% | Remainder |
|  | Chromium, Cr | 0.04–0.35% | 0.04–0.35% | |
|  | Copper, Cu | 0.15–0.40% | 0.15–0.40% | |
|  | Iron, Fe | ≤0.70% | ≤0.70% | |
|  | Magnesium, Mg | 0.80–1.2% | 0.80–1.2% | |
|  | Manganese, Mn | ≤0.15% | ≤0.15% | |
|  | Silicon, Si | 0.40–0.80% | 0.40–0.80% | |
|  | Titanium, Ti | ≤0.15% | ≤0.15% | |
|  | Zinc, Zn | ≤0.25% | ≤0.25% | |

Our Blog

## View our latest news

[![The Key Differences Between UHMW and HDPE Plastic Machining](https://hplmachining.com/wp-content/uploads/2025/01/3.6.png)](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

[January 9, 2025](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

[The Key Differences Between UHMW and HDPE Plastic Machining](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

The importance of plastic machining in industries that require precision-engineered components cannot be overemphasized; it is among the most versatile materials for such applications. Both plastics have similar features;...

[Read More](https://hplmachining.com/blog/what-is-the-difference-between-uhmw-and-hdpe-machining/)

[![3.1 1](https://hplmachining.com/wp-content/uploads/2025/01/3.1-1.webp)](https://hplmachining.com/blog/what-is-cnc-milling/)

[January 9, 2025](https://hplmachining.com/blog/what-is-cnc-milling/)

[Everything You Need to Know About CNC Milling: How a CNC Mill Works](https://hplmachining.com/blog/what-is-cnc-milling/)

The CNC milling machine is an advanced manufacturing method that offers unique accuracy, productivity, and flexibility in making complicated parts and elements. Nevertheless, what is a CNC mill? Furthermore,...

[Read More](https://hplmachining.com/blog/what-is-cnc-milling/)

[![Why Are CNC Machines Important in Modern Manufacturing?](https://hplmachining.com/wp-content/uploads/2025/01/4.1.webp)](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

[January 9, 2025](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

[Understanding the Key Components of a CNC Machine](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

Modern manufacturing has been changed by CNC (Computer Numerical Control) machines that give unmatched efficiency, precision, and flexibility. Experts in the field or beginners in automated machining need to...

[Read More](https://hplmachining.com/blog/parts-of-a-cnc-machine/)

[![Unlocking the Mysteries: The Key Differences Between Metal Cutting and Machining Processes](https://hplmachining.com/wp-content/uploads/2025/01/1-12.webp)](https://hplmachining.com/blog/cutting-and-machining-metal/)

[January 9, 2025](https://hplmachining.com/blog/cutting-and-machining-metal/)

[Unlocking the Mysteries: The Key Differences Between Metal Cutting and Machining Processes](https://hplmachining.com/blog/cutting-and-machining-metal/)

In the shaping and fabrication of metallic materials, there is a need to differentiate between metal cutting processes and machining processes for both industry professionals and amateurs. These two...

[Read More](https://hplmachining.com/blog/cutting-and-machining-metal/)

![Get 6061 aluminum CNC machining parts from Hopeful](https://hplmachining.com/wp-content/uploads/2025/01/2-10.webp)

## Get 6061 aluminum CNC machining parts from Hopeful

Hopeful Company specializes in producing 6061 aluminium CNC machined parts, which are well known for their durability, accuracy and strength. We can manufacture standard or customized products according to your specifications using the latest CNC machines and experienced personnel. Call us now and enjoy great products plus excellent customer service.

[Get an Instant Quote](#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjE2OTQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D)

Scroll to Top

WhatsApp us

Get in touch with Kunshan Hopeful Metal Products Co.,Ltd

Contact Form used

Your Name \*

Email

Phone/WhatsApp

Your Message

File Upload

Please upload your processing drawings, we promise that the uploaded files will be confidential

Submit Form

```json
{"@context":"https://schema.org","@graph":[{"@type":"BreadcrumbList","@id":"https://hplmachining.com/services/cnc-machining/aluminum/6061-t6/#breadcrumb","itemListElement":[{"@type":"ListItem","position":"1","item":{"@id":"https://hplmachining.com","name":"Home"}},{"@type":"ListItem","position":"2","item":{"@id":"https://hplmachining.com/services/","name":"Services"}},{"@type":"ListItem","position":"3","item":{"@id":"https://hplmachining.com/services/cnc-machining/","name":"CNC Machining Service"}},{"@type":"ListItem","position":"4","item":{"@id":"https://hplmachining.com/services/cnc-machining/aluminum/","name":"Aluminum CNC Machining Service"}},{"@type":"ListItem","position":"5","item":{"@id":"https://hplmachining.com/services/cnc-machining/aluminum/6061-t6/","name":"Aluminum 6061"}}]}]}
```